Measurement Background
Pitting corrosion as the initial stage of corrosion damage, is due to the metal surface in the tensile stress or the role of chemical substances, due to the destruction of the protective layer and the emergence of local penetration, so that the metal substrate is directly exposed to the corrosive environment to form local corrosion of small holes and to the depth of the development of a form of corrosion damage. Usually pitting corrosion occurs in the region easy to form a source of fatigue. Pitting corrosion on the surface of the structure to form corrosion pits to change the surface state of the structure, which in turn led to a local or comprehensive damage.

The structure of metal materials by the role of the medium and the state of change in the formation of a new phase of corrosion damage, and corrosion damage to the national economy and national defence construction of the harm is very serious, not only will lead to production standstill, material and structural failures, resource loss, leakage of hazardous substances, etc., but also may lead to significant economic losses or even catastrophic consequences. Countries around the world every year to invest a lot of human and material resources for corrosion detection and protection, corrosion detection has become one of the important areas of modern scientific and technological research, timely and accurate discovery of corrosion damage and assessment of the extent of its damage to the safety of metal materials and structures and the economy is of great significance.

Why Choose Ultrasonic Thickness Measurement as Method of Inspection
Inspectors perform non-destructive testing of in-service pipelines and boilers in the petroleum, chemical, and natural gas industries to assess the degree of wall thickness reduction and to estimate the remaining life cycle of the equipment. The use of high precision ultrasonic thickness gauges to measure the wall thickness of pipelines is a very effective and accurate way to do this. Inspectors can anticipate the possibility of pitting before the pipe is seriously corroded, so that repairs and maintenance can be carried out in advance, thus extending the life of the pipe.
Tested Sample
We received an email from an oilfield company, they asked whether our products in the measurement of oil pipeline wall thickness at the same time whether it is possible to detect pitting defects with a diameter of more than 1mm in advance, we mentioned the user's thickness measurement needs for a special production of pitting corrosion comparison test block, the actual wall thickness of the pitting test block is 8mm, in the bottom of the sample block were produced for the diameter of the 6 artificial defects, the bottom of the test block style is as follows The depth of the artificial defects on the upper surface of the test block from left to right is 6.9, 6.1, 5.1, 3.9, 3.1, 2.1 mm.

Measurement Anaysis
1.Defect free
Using ultrasonic thickness gauge to detect small-diameter point defects and can accurately identify the specific location of the defect is very difficult, which requires the instrument has very high detection resolution and accuracy, and need to have A-scan real-time function, can clearly show the defects' bottom echo, so we chose to use the PM5 Gen2 ultrasonic thickness gauge with A-scan real-time display in the direction of the front of the test block for testing, when the measurement of no defects, in addition to the interface reflection wave is only acquired on the bottom surface of the sample reflective waveform, as shown in the figure below:

2.Defective
When the probe is placed directly above the artificial defects, the waveform can be seen through the waveform in front of the reflection wave on the bottom surface of the sample block there is a set of defects in the reflection waveform, then the waveform of the defective wave is obtained and the depth and location of the defective wave is displayed, as shown below the waveform of the red circle for the reflection wave of defect.


Summary
Through the above test experiments found that YUSHI PM5Gen2 ultrasonic thickness gauge can distinguish the defect diameter of 1mm pitting defects, for oil, natural gas pipeline wall thickness inspection not only to measure the wall thickness, but also helps you to find out in advance that the pipeline may exist a very small pitting defects, pipeline repair in a timely manner has great significance!